HASTELLOY B-3 UNS N10675/W.Nr.2.4600
| Paduan | unsur | C | Si | Mn | S | P | Ni | Cr | Mo | Fe | Co | Cu | Al | W |
| PaduanB3 | Menit | 1.0 | 28.5 | 1.6 | ||||||||||
| Maks. | 0.01 | 0.08 | 3.00 | 0.01 | 0.02 | 65.0 | 3.0 | 30.0 | 2.0 | 3.0 | 1.0 | 0.1 | 3.0 |
| Status Aolly | Kakuatan regangan Rm MpaMin | Kakuatan ngahasilkeun RP 0.2MpaMin | Pemanjangan 5%Min |
| Ssolusi | 760 | 350 | 40 |
| Kapadetang/cm3 | Titik Lebur℃ |
| 9.22 | 1370~1418 |
Batang, Batang, Kawat sareng Bahan Tempa -ASTM B 335 (Rod, Bar), ASTM B 564 (Tempaan,flens)
Pelat, Lambaran sareng Strip- ASTM B 333
Pipa jeung Tabung -ASTM B 622 (Mulus) ASTM B 619/B626 (Tabung Dilas)
● Ngajaga daktilitas anu saé nalika paparan samentawis kana suhu sedeng
● Résistansi anu saé pisan kana retakan bolong, korosi sareng korosi setrés
● Résistansi anu saé pisan kana serangan péso sareng zona anu kapangaruhan ku panas
● Résistansi anu saé pisan kana asam asétat, format sareng fosfat sareng média non-oksidasi anu sanés
● Résistansi kana asam klorida dina sadaya konsentrasi sareng suhu
● Stabilitas termal langkung unggul tibatan paduan B-2